Multibase Multi-Flex® TPO D 6713

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Multibase
Trade Name Multi-Flex® TPO
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPO D 6713.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792-91
Melt Flow 10 g/10 min
10 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 67
67
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate 16.5 MPa
2390 psi
ASTM D638-95
Elongation at Break 70 %
70 %
ASTM D638-95
Flexural Strength 26.9 MPa
3900 psi
ASTM D790-95
Flexural Modulus 1.275 GPa
184.9 ksi
Method 1, Proc. B; ASTM D-790-95
Tear Strength 93.0 kN/m
531 pli
ASTM D624-95
Users viewing this material also viewed the following: