Material Notes:
Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
Physical Properties Metric English Comments
Ash 24.46 %
24.46 %
ISO 3451/1
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.147 J/cm
0.275 ft-lb/in
73°F; ISO 180
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 128 °C
262 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C
162 °F
Unannealed; ASTM D648
Flame Spread 7.9 mm/min
0.31 in/min
ISO 3795