Multibase Multibatch® MP 52214 Injection Molding

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Multibase
Trade Name Multibatch®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multibatch® MP 52214 Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HPP. 75% CaCO3, 10%TiO2FilledFine Particle Size.Information provided by Multibase
Physical Properties Metric English Comments
Density 1.81 g/cc
0.0654 lb/in³
ISO R 1183
Melt Flow 35 g/10 min

@Load 5.00 kg,
Temperature 230 °C
35 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133