Multibase Multibatch® MP 52659 Sheet Extrusion

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Multibase
Trade Name Multibatch®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multibatch® MP 52659 Sheet Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HPP. 60% Talc Filled.Lamellar talcInformation provided by Multibase
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ISO R 1183