NCMT NanoPAC™ S212 High Performance Polypropylene Nanocomposite

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Nano Composite Materials Technology Ltd
Trade Name NanoPAC™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NCMT NanoPAC™ S212 High Performance Polypropylene Nanocomposite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: High stiffness Supplementary of ABS Good impact resistant Less shrinkage Good thermal conductivity Applications: Toys Industry AutomobileInformation provided by Nano Composite Materials Technology Limited
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
NCMT Method
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 20.0 MPa
2900 psi
ASTM D638
Elongation at Break >= 500 %
>= 500 %
ASTM D638
Tensile Modulus 2.00 GPa
290 ksi
ASTM D638
Izod Impact, Notched 2.70 J/cm
5.06 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 110 °C
230 °F
Deflection Temp.; ASTM D648