Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NCMT NanoPAC™ S216 High Performance Polypropylene Nanocomposite

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Nano Composite Materials Technology Ltd
Trade Name NanoPAC™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NCMT NanoPAC™ S216 High Performance Polypropylene Nanocomposite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics: High stiffness Supplementary of ABS Good impact resistant Less shrinkage Good thermal conductivity Applications: Toys Industry AutomobileInformation provided by Nano Composite Materials Technology Limited
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
NCMT Method
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 19.0 MPa
2760 psi
ASTM D638
Elongation at Break >= 600 %
>= 600 %
ASTM D638
Tensile Modulus 2.10 GPa
305 ksi
ASTM D638
Izod Impact, Notched 5.00 J/cm
9.37 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 110 °C
230 °F
Deflection Temp.; ASTM D648
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved