Material Notes:
Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product to obtain mechanical properties for form molding parts with a thickness over 10 mm.Information provided by NOVA Chemicals.
Physical Properties Metric English Comments
Bulk Density 0.580 - 0.640 g/cc
0.0210 - 0.0231 lb/in³
Of unexpanded product
0.610 g/cc
0.0220 lb/in³
Typical; unexpanded product
Density 0.0170 - 0.0350 g/cc
0.000614 - 0.00126 lb/in³
Usual Use