Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nanocyl PLASTICYL™ PA1503 Polyamide 6 with - Carbon Nanotube Masterbatch

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Carbon Fiber Filled
Manufacturer Nanocyl
Trade Name PLASTICYL™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nanocyl PLASTICYL™ PA1503 Polyamide 6 with - Carbon Nanotube Masterbatch.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLASTICYL™ PA1503 is a conductive masterbatch based on polyamide 6. Because of its high flow formulation, PLASTICYL™ PA1503 is ideal for standard injection molding and extrusion processes.Applications:ESD (Electrostatic Discharge) and electrically conductive partsE&E, automotive, industrialInjection molding, extrusionBenefits:Electrical conductivity at low loadingRetention of key mechanical propertiesEasier processing
Physical Properties Metric English Comments
Specific Gravity 1.175 g/cc
1.175 g/cc
ISO 1183
Filler Content 14 - 16 %
14 - 16 %
Carbon Nanotube Loading
High Load Melt Index <= 3.16 g/10 min

@Load 20.0 kg,
Temperature 280 °C
<= 3.16 g/10 min

@Load 44.1 lb,
Temperature 536 °F
4 mm; Non-standard Test
Thermal Properties Metric English Comments
Melting Point 221 °C
430 °F
ISO 11357-1,-3