Material Notes:
Description: Natural PolycarbonateInformation provided by Network Polymers Inc.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Water Absorption 0.15 %
0.15 %
24 hours at 73°F; ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Yield 71.0 MPa
10300 psi
chs 2 in/min; ASTM D638
Flexural Strength 96.5 MPa
14000 psi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Flexural Modulus 2.41 GPa
350 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
Test Method A (0.125 in bar); ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
260 °F
0.125 in bar; ASTM D648
Flammability, UL94 V-2
V-2
0.062 in, All Colors