Niche Polymer ABSN3BK ABS

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer Niche Polymer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Niche Polymer ABSN3BK ABS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Niche Polymer
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00600 cm/cm
0.00600 in/in
ASTM D955
Melt Flow 8.00 g/10 min

@Load 3.80 kg,
Temperature 230 °C
8.00 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D123
Mechanical Properties Metric English Comments
Tensile Strength at Break 45.0 MPa
6530 psi
ASTM D638
Elongation at Break 2.00 %
2.00 %
ASTM D638
Flexural Strength 77.2 MPa
11200 psi
ASTM D790
Flexural Modulus 2.34 GPa
339 ksi
ASTM D790
Izod Impact, Unnotched 1.60 J/cm

@Thickness 3.17 mm
3.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 94.00 °C
201.2 °F
ASTM D648
Descriptive Properties Value Comments
Color Black