Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Nitriflex N-6011 NBR - Nitrile Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Nitriflex
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nitriflex N-6011 NBR - Nitrile Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent for extruded, low die swell, high tensile strength, excellent compression set properties. Applications: Printing rolls with low hardness, gaskets, blankets, rice dehusking roller, friction materials. Information provided by Dax Resinas
Physical Properties Metric English Comments
Volatiles 0.00 - 0.70 %
0.00 - 0.70 %
Method B-003; ASTM D5668
Mooney Viscosity 110 - 120

@Temperature 100 °C
110 - 120

@Temperature 212 °F
MML1+4, Method B-002; ASTM D1646
Ash 0.00 - 1.0 %
0.00 - 1.0 %
Method B-007; ASTM D5667
Descriptive Properties Value Comments
Appearance Light beige to yellowish
Bound Acrylonitrile Content (%) 31 - 34
ASTM D3533
Polymerization Cold