Material Notes:
Good processability, elasticity at low temperature, moderate oil resistance and low mold fouling. Applications: fuel hose packing, gaskets, diaphragms. Information provided by Dax Resinas
Physical Properties Metric English Comments
Volatiles 0.00 - 0.70 %
0.00 - 0.70 %
Method B-003; ASTM D5668
Mooney Viscosity 40 - 55

@Temperature 100 °C
40 - 55

@Temperature 212 °F
ML1+4, Method B-002; ASTM D1646
Ash 0.00 - 0.50 %
0.00 - 0.50 %
ASTM D5667
Descriptive Properties Value Comments
Appearance White to yellowish
Bound Acrylonitrile Content (%) 26 - 28
ASTM D3533
Polymerization Cold