Northstar Polymers MNA-014 Prepolymer

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Liquid
Manufacturer Northstar Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Northstar Polymers MNA-014 Prepolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Northstar Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.218 g/cc
1.218 g/cc
Descriptive Properties Value Comments
Equivalent Weight 144.5
NCO (%) 29