Information provided by Northstar Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.204 g/cc
1.204 g/cc
Viscosity 60 cP

@Temperature 82.2 °C
60 cP

@Temperature 180 °F
1000 - 1200 cP

@Temperature 21.7 °C
1000 - 1200 cP

@Temperature 71.0 °F
Descriptive Properties Value Comments
Amine Equivalents 183
Appearance at 25°C Liquid, Amber Colored
NCO (%) 23