Northstar Polymers SBA-021 Polyester Curing Agent

Category Polymer , Thermoset , Polyester, TS
Manufacturer Northstar Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Northstar Polymers SBA-021 Polyester Curing Agent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Northstar Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.134 g/cc
1.134 g/cc
Descriptive Properties Value Comments
Appearance at 25°C White Waxy Solid
Equivalent Weight 206