Nye Lubricants 570H-2 (NT) Synthetic Oil

Category Fluid , Lubricant , Perfluoropolyether (PFPE) , Silica Gellant
Manufacturer Nye Lubricants
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nye Lubricants 570H-2 (NT) Synthetic Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Viscosity Measurement 144
144
Viscosity Index of Base Oil; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 500 cSt
500 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 43 cSt
43 cSt
Base Oil; ASTM D445
Evaporation Loss 1.0 %
1.0 %
6.5 hrs, 200C; ASTM D972
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 225 °C
437 °F
Recommended
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Recommended
Pour Point -28.0 °C
-18.4 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type PFPE(pnd)
Gellant Type Silica(BL)