Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Viscosity Measurement 152
152
Viscosity Index of Base Oil; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 194 cSt
194 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 23 cSt
23 cSt
Base Oil; ASTM D445
Evaporation Loss 0.18 %
0.18 %
24 hrs, 100C; ASTM D972
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 260
260
ASTM D217
Penetration P(60), 1/10 mm 281
281
ASTM D217
Oil Separation 3.0 %
3.0 %
24 hrs, 100C; FTM 719B, 321.2
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Recommended
Minimum Service Temperature, Air -34.0 °C
-29.2 °F
Recommended
Pour Point -40.0 °C
-40.0 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type PAO
Gellant Type Silica (WL)