Nye Lubricants 713 (NG) Synthetic Oil

Category Fluid , Lubricant , Silica Gellant
Manufacturer Nye Lubricants
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nye Lubricants 713 (NG) Synthetic Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 160 cSt
160 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 7.8 cSt
7.8 cSt
Base Oil; ASTM D445
Evaporation Loss 4.5 %
4.5 %
24 hrs, 100C; ASTM D972
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 271
271
ASTM D217
Penetration P(60), 1/10 mm 280
280
ASTM D217
Oil Separation 7.7 %
7.7 %
24 hrs, 100C; FTM 719B, 321.2
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 250 °C
482 °F
Recommended
Minimum Service Temperature, Air 0.000 °C
32.0 °F
Recommended
Pour Point -6.00 °C
21.2 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type CTFE
Gellant Type Silica (WL)