Nye Lubricants 774VHF-MS (NG) Synthetic Oil

Category Fluid , Lubricant , Polyalphaolefin (PAO) , Silica Gellant
Manufacturer Nye Lubricants
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nye Lubricants 774VHF-MS (NG) Synthetic Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Viscosity Measurement 323
323
Viscosity Index of Base Oil; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 16800 cSt
16800 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 1380 cSt
1380 cSt
Base Oil; ASTM D445
Evaporation Loss 0.10 %
0.10 %
24 hrs, 100C; ASTM D972
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 225
225
ASTM D217
Penetration P(60), 1/10 mm 220
220
ASTM D217
Oil Separation 0.20 %
0.20 %
24 hrs, 100C; FTM 719B, 321.2
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Recommended
Minimum Service Temperature, Air -10.0 °C
14.0 °F
Recommended
Pour Point -17.0 °C
1.40 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type PAO
Gellant Type Silica (WL)