Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Viscosity Measurement 210
210
Viscosity Index of Base Oil; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 513 cSt
513 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 79 cSt
79 cSt
Base Oil; ASTM D445
Evaporation Loss 0.00 %
0.00 %
24 hrs, 150C; ASTM D972
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 312
312
ASTM D217
Penetration P(60), 1/10 mm 305
305
ASTM D217
Oil Separation 3.0 %
3.0 %
24 hrs, 150C; FTM 719B, 321.2
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Recommended
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Recommended
Pour Point -40.0 °C
-40.0 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type Sil.(Fluor)
Gellant Type PTFE
Users viewing this material also viewed the following: