Nye Lubricants UniFlor 8711 (UF) Synthetic Oil

Category Fluid , Lubricant , Perfluoropolyether (PFPE) , PTFE Gellant
Manufacturer Nye Lubricants
Trade Name UniFlor
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nye Lubricants UniFlor 8711 (UF) Synthetic Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Viscosity Measurement 171
171
Viscosity Index of Base Oil; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 26 cSt
26 cSt
Base Oil; ASTM D445
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
6.0 cSt
Base Oil; ASTM D445
Evaporation Loss 0.70 %
0.70 %
24 hrs, 100C; ASTM D972
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 276
276
ASTM D217
Penetration P(60), 1/10 mm 288
288
ASTM D217
Oil Separation 8.0 %
8.0 %
24 hrs, 100C; FTM 719B, 321.2
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Recommended
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Recommended
Pour Point -76.0 °C
-105 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type PFPE(lin)
Gellant Type PTFE