Nye Lubricants UniFlor 8955 (UF) Synthetic Oil

Category Fluid , Lubricant , Perfluoropolyether (PFPE) , Zinc Oxide Gellant
Manufacturer Nye Lubricants
Trade Name UniFlor
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Nye Lubricants UniFlor 8955 (UF) Synthetic Oil.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Nye Lubricants.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 18 cSt
18 cSt
Base Oil; ASTM D445
Evaporation Loss 0.20 %
0.20 %
24 hrs, 100C; ASTM D972
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 280
280
ASTM D217
Oil Separation 4.1 %
4.1 %
24 hrs, 100C; FTM 719B, 321.2
Thermal Properties Metric English Comments
Pour Point -90.0 °C
-130 °F
Base Oil; ASTM D97
Descriptive Properties Value Comments
Base Fluid Type PFPE(lin)
Gellant Type Zinc Oxide