Material Notes:
Description: Nylene® NX4747 is a 14% glass fiber reinforced translucent specialty nylon. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.23 g/cc
1.23 g/cc
ASTM D792
Viscosity Measurement 30
30
relative viscosity, FAV
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 124 MPa
18000 psi
ASTM D638
Elongation at Break 3.5 %
3.5 %
ASTM D638
Flexural Modulus 5.31 GPa
770 ksi
ASTM D790
Izod Impact, Notched 0.694 J/cm
1.30 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 210 °C
410 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 188 °C
370 °F
ASTM D648