Ohio Carbon Blank OCB UT-3 Mechanical Grade Graphite

Category Carbon , Graphite
Manufacturer Ohio Carbon Blank
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ohio Carbon Blank OCB UT-3 Mechanical Grade Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in a range of sizes and shapes.
Physical Properties Metric English Comments
Apparent Bulk Density 1.70 g/cc
0.0614 lb/in³
Particle Size 10.2 µm
10.2 µm
Average
Mechanical Properties Metric English Comments
Hardness, Shore D 50
50
Tensile Strength 20.7 MPa
3000 psi
Flexural Strength 36.5 MPa
5300 psi
Compressive Strength 68.9 MPa
10000 psi
Thermal Properties Metric English Comments
Thermal Conductivity 93.4 W/m-K
648 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.00135 ohm-cm
0.00135 ohm-cm
Descriptive Properties Value Comments
Grain Fine
Suggested Applications Forging Dies
Large Cavity Molds
Large Die Casts
Large Extrusion Dies
Roughing Electrodes