Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ovation Polymers Opnyl OP66GF43 Nylon 66, As Conditioned

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Ovation Polymers
Trade Name Opnyl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers Opnyl OP66GF43 Nylon 66, As Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nylon 66-Glass reinforced(43%), high tensile strength, stiffness and HDT.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.52 g/cc
1.52 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 230 MPa
33400 psi
50 mm/min; ASTM D638
Elongation at Break 2.8 %
2.8 %
50 mm/min; ASTM D638
Tensile Modulus 9.00 GPa
1310 ksi
50 mm/min; ASTM D638
Flexural Yield Strength 250 MPa
36300 psi
1.3 mm/min; ASTM D790
Flexural Modulus 11.0 GPa
1600 ksi
1.3 mm/min; ASTM D790
Izod Impact, Notched 1.068 J/cm

@Temperature 23.0 °C
2.001 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 253 °C

@Thickness 3.20 mm
487 °F

@Thickness 0.126 in
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 247 °C

@Thickness 3.20 mm
477 °F

@Thickness 0.126 in
ASTM D648
Users viewing this material also viewed the following: