Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ovation Polymers Opnyl OP6MT254 Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Ovation Polymers
Trade Name Opnyl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ovation Polymers Opnyl OP6MT254 Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nylon 6 – Mighty Tough plasticized extrusion grade for tubing/profile applications. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Variations within normal tolerances are possible for various types of colors and functional properties like UV resistance.Information provided by Ovation Polymers
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Melt Index of Compound 4.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
50 mm/min; ASTM D638
Elongation at Break 60 %
60 %
50 mm/min; ASTM D638
Flexural Yield Strength 20.0 MPa
2900 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 0.700 GPa
102 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Melting Point 220 - 222 °C
428 - 432 °F
DSC @ 15°C/min; ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 64.0 °C

@Thickness 3.20 mm
147 °F

@Thickness 0.126 in
Unannealed; ASTM D648
Users viewing this material also viewed the following: