Material Notes:
Good resistance to heat and moderate chemicals and moderate resistance to oils. Has good characteristics to resist sea water, acids, fats, greases and many solvents. Neoprene has good ozone resistance and flame retardant properties.Information provided by P & P Technology
Physical Properties Metric English Comments
Specific Gravity 0.110 - 0.150 g/cc
0.110 - 0.150 g/cc
Water Absorption 5.0 %
5.0 %
Deformation 25 %

@Pressure 0.0350 - 0.0630 MPa
25 %

@Pressure 5.08 - 9.14 psi
Mechanical Properties Metric English Comments
Hardness, Shore D 40
40
base rubber
Tensile Strength 0.450 MPa
65.3 psi
Elongation at Break 150 %
150 %
Compression Set <= 10 %

@Temperature 23.0 °C,
Time 86400 sec
<= 10 %

@Temperature 73.4 °F,
Time 24.0 hour
0.5
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 80.0 °C
176 °F
continuous
100 °C
212 °F
intermittent
Minimum Service Temperature, Air -34.0 °C
-29.2 °F
Descriptive Properties Value Comments
Color Black