Palm Labs Adhesives TURBO FUSE SERIES 110 MEDICAL DEVICES APPROVED (5 Viscosity) Rapid Bonding Adhesive

Category Polymer , Adhesive
Manufacturer Palm Labs Adhesives
Trade Name TURBO FUSE SERIES
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Palm Labs Adhesives TURBO FUSE SERIES 110 MEDICAL DEVICES APPROVED (5 Viscosity) Rapid Bonding Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Palm Lab's cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 110 MEDICAL DEVICES APPROVED advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performance has been tested with a variety of materials, and is recommended for a multitude of applications. The fast curing qualities make it especially desirable in high speed industrial production. TURBO FUSE MEDICAL DEVICES APPROVED is ideal for use in applications that require good "wicking" characteristics and/or in close fitting applications approved for use on Medical Devices. Because of TurboFuse 110 Series low viscosity, it works especially well in close fitting applications such as metal to metal bonding, and rubber to rubber such as "O" ring repair/manufacture.Part Numbers for this data: 04-110M, 10-110M, 15-110M, 20-110M, 25-110M, 30-110MSoluble in Acetone, MEK, Amide, Methylene ChlorideInformation provided by Palm Laboratories Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
Liquid State
Viscosity 2.0 - 5.0 cP
2.0 - 5.0 cP
Liquid State
Mechanical Properties Metric English Comments
Hardness, Barcol 65
65
Cured State
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.2 °C
180 °F
Cured State
Softening Point 149 °C
300 °F
Cured State
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Cured State
Flash Point 76.7 - 93.3 °C
170 - 200 °F
Liquid State
Electrical Properties Metric English Comments
Dielectric Constant 3.33

@Frequency 1.00e+6 Hz
3.33

@Frequency 1.00e+6 Hz
Cured State
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Liquid State
Descriptive Properties Value Comments
Appearance Clear Liquid
Liquid State
Clear-Hard
Cured State
Base compound (Resin) Ethyl Cyanoacrylate
Liquid State
Gap Fill 0.002"
Cured State
Material Set Up Time <3 sec
Rubber to Rubber
3-10 sec
Polycarbonate to Polycarbonate
3-5 sec
Phenolic to Phenolic
3-5 sec
Aluminum to Aluminum
5-15 sec
Steel to Steel