Parker Chomerics CHO-SHIELD® 610 Part C Solvent Blend

Category Polymer , Adhesive
Manufacturer Parker Chomerics
Trade Name CHO-SHIELD®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-SHIELD® 610 Part C Solvent Blend.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity <= 1.00 g/cc
<= 1.00 g/cc
Volatiles 100 %
100 %
Descriptive Properties Value Comments
Isopropanol wt. % max 15 - 25
Methyl Ethyl Ketone wt. % 40 - 50
n-Butyl Alcohol wt. % 30 - 40
Physical Form Clear liquid with solvent odor
Solubility in Water Partially