Parker Chomerics CHO-SHIELD® 611 Part B Coating Catalyst

Category Other Engineering Material , Catalyst/Initiator , Polymer , Adhesive
Manufacturer Parker Chomerics
Trade Name CHO-SHIELD®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-SHIELD® 611 Part B Coating Catalyst.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity <= 1.00 g/cc
<= 1.00 g/cc
Volatiles 80 %
80 %
Descriptive Properties Value Comments
Butanol wt. % Max 10
Ethyl Benzene wt. % Max 5
Isopropanol wt. % max 5
Methyl isobutyl ketone wt. % Max 45
Physical Form Dark amber liquid
Polyamide Resin wt. % Max 25
Xylene wt. % 20 - 30