Pau Tai Avanstab HP-235 Organotin Stabilizer Octyl Thiotins/Methyl Thiotin

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Pau Tai Industrial Corp.
Trade Name Avanstab
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pau Tai Avanstab HP-235 Organotin Stabilizer Octyl Thiotins/Methyl Thiotin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Is a multifunctional lubricant/tin one-pack system stabilizer.Designed for PVC rigid pipe extrusion in multiscrew extruders at typical use levels of 2.0-2.5 phr.Avanstab HP-235 provides more homogenous compounding and excellent color hold.Its chemical composition meet the specifications of NSF approved for potable water pipe.Information provided by Pau Tai Industrial Corp.