Pau Tai Unistab BT-11 Organotin Stabilizer Butyl/Octyl Carboxylate Tin

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Pau Tai Industrial Corp.
Trade Name UNISTAB
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pau Tai Unistab BT-11 Organotin Stabilizer Butyl/Octyl Carboxylate Tin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Is di-butyl tin di-laurate,excellent clarity lubricity and heat stability.It is an effective catalyst for polyurethane,silicone and many cross-linkable polymers.Information provided by Pau Tai Industrial Corp.