Pau Tai Unistab BT-53C Mixed Metal Liquid Stabilizer for PVC Cadmium/Barium/Zinc Self-Lubricating

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Pau Tai Industrial Corp.
Trade Name UNISTAB
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pau Tai Unistab BT-53C Mixed Metal Liquid Stabilizer for PVC Cadmium/Barium/Zinc Self-Lubricating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Is a high performance low odor butyl tin maleate stabilizer,recommended for all rigid colar outdoor applications,such as constrction sheets and profiles,when maximum light and weathering stability is required.Information provided by Pau Tai Industrial Corp.