Polimeri Europa Dutral® PM 06 PLE Ethylene - Propylene Masterbatch

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Dutral®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Dutral® PM 06 PLE Ethylene - Propylene Masterbatch.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dutral® PM 06 PLE is a masterbatch based on Ethylene - Propylene elastomer produced by suspension polymerization using a Ziegler-Natta Catalyst. A non-staining antioxidant is added during the production process.Key Features: Dutral® elastomers are characterized by excellent resistance to ageing and weathering, good resistance to both high an low temperatures, low permanent set values, good resistance to a large number of chemicals. Dutral® PM 06 PLE is a masterbatch suitable for polyolefin modification, especially low flow PP(MFI (230°C/2.16kg) = 1-10 g/10 mins).Main Applications: Polymer modification.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Volatiles <= 0.20 %
<= 0.20 %
Melt Flow 1.8 g/10 min

@Load 5.00 kg,
Temperature 230 °C
1.8 g/10 min

@Load 11.0 lb,
Temperature 446 °F
Ash <= 0.30 %
<= 0.30 %
Descriptive Properties Value Comments
Pellets Size 0.45 g
wt of 30 pellets