Polimeri Europa Europrene Latice® 5595 Carboxylated Styrene - Butadiene Copolymer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Styrene Butadiene Rubber
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Europrene Latice®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Europrene Latice® 5595 Carboxylated Styrene - Butadiene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Europrene Latice® 5595 is an aqueous dispersion of a carboxylated styrene-butadiene copolymer obtained using synthetic anionic emulsifiers.Key Features: Europrene Latice® 5595 is specifically designed to obtain high porosity and extremely good runnability.Main Applications: Europrene Latice® 5595 is used for offset and web-offset paper and board coating.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Solids Content 50 %
50 %
Total; ASTM D1417
pH 7.0
7.0
ASTM D1417
Brookfield Viscosity 400 cP
400 cP
20 rpm; ASTM D1417
Surface Tension 40 dynes/cm
40 dynes/cm
ASTM D1417