Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Europrene® SOL TH 2315 Styrene - Ethylene / Butylene Block Copolymer

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Europrene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Europrene® SOL TH 2315 Styrene - Ethylene / Butylene Block Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Europrene® SOL TH 2315 is a linear block copolymer obtained by selective hydrogenation of styrene-butadiene-styrene block copolymers. The polymer is based on styrene and ethylene/butylene, where bound styrene content is 32%wt. A non-staining, TNPP free antioxidant system is added during the production process.Key Features: Europrene® SOL TH 2315 is a linear triblock copolymer of high molecular weight, specifically designed to be formulated with high contents of processing oils and mineral fillers. The grade is characterized by excellent mechanical properties and ageing resistance.Main Applications: Europrene® SOL TH 2315 is designed for technical compound applications. High performance compounds base on Europrene® SOL TH 2315 show excellent elastic and tensile characteristics, in a wide range of flowability and hardness.Information provided by Polimeri Europa. Mechanical properties measured on ASTM D 4703 compression molded samples.
Physical Properties Metric English Comments
Melt Flow <= 1.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
<= 1.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 68
68
ASTM D2240
Tensile Strength at Break 25.0 MPa
3630 psi
ASTM D412
Elongation at Break 600 %
600 %
ASTM D412
300% Modulus 0.00350 GPa
0.508 ksi
ASTM D412