Material Notes:
AquaGard products are designed to improve the flame retardency of polyolefins without the use of halogen additives, such as bromine or chlorine. AquaGard products are available in a polyethylene or polypropylene carrier, and typically comply with UL94 fire and smoke regulations. Several grades are available, or Aguagard can be specifically formulated to satisfy individual requirements.Information provided by the manufacturer, PolyChemAlloy.
Physical Properties Metric English Comments
Specific Gravity 1.20 - 1.30 g/cc
1.20 - 1.30 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore D 38 - 42
38 - 42
Elongation at Yield 340 - 360 %
340 - 360 %
Thermal Properties Metric English Comments
Oxygen Index 33 %
33 %
Electrical Properties Metric English Comments
Dissipation Factor 0.00015

@Frequency 2.00e+9 Hz
0.00015

@Frequency 2.00e+9 Hz
Processing Properties Metric English Comments
Processing Temperature <= 230 °C
<= 446 °F
Keep below 250°C (482°F) to optimize flame retardant performance.
Descriptive Properties Value Comments
Active Content 30 wt.%
Carrier Polyethylene
Color White
Custom colors available