PolyChem Alloy HydroBond 4000F

Category Polymer
Manufacturer PolyChem Alloy
Trade Name HydroBond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyChem Alloy HydroBond 4000F.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A Proprietary multi-component system used for wood bonding applications requiring heat and water resistance. Comes in a liquid paste form and is available in a variety of colors.
Physical Properties Metric English Comments
pH 3.8 - 4.8
3.8 - 4.8
Descriptive Properties Value Comments
Color White
Various colors available