PolyOne Edgetek® NL-50GF/000 Black 13 Nylon 6/12, Glass Filled  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 612
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® NL-50GF/000 Black 13 Nylon 6/12, Glass Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Glass Fiber ReinforcedHeat StabilizedBlackNylon 6/12 CompoundDry as Molded:PolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.52 g/cc
1.52 g/cc
ASTM D792
Water Absorption 0.20 %
0.20 %
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 200 MPa
29000 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 2.0 %
2.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus 11.7 GPa
1700 ksi
ASTM D790
Izod Impact, Notched 1.55 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
2.90 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
Annealed, 0.125 in bars; ASTM D648