Description/Features:Glass Bead FilledUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 13.1 MPa
1900 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 1.0 %
1.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 1.282 GPa
185.9 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 58.6 MPa
8500 psi
ASTM D790
Flexural Modulus 1.28 GPa
186 ksi
ASTM D790
Izod Impact, Notched 0.641 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.20 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Processing Properties Metric English Comments
Melt Temperature 210 - 232 °C
410 - 450 °F
Molding
Mold Temperature 48.9 - 71.1 °C
120 - 160 °F
Descriptive Properties Value Comments
Product Form Pellets