Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Unreinforced, Molded
Manufacturer PolyOne Corporation
Trade Name Edgetek®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® XT XT-100-BW00 Natural Polycarbonate + PBT (PC+PBT).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of general purpose, UV stable and low-temperature impact grades for use in a wide range of demanding applications and severe operating environments plus customized formulations to meet specialized requirements.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 56.5 MPa
8190 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 120 %
120 %
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 82.7 MPa
12000 psi
ASTM D790
Flexural Modulus 2.17 GPa
315 ksi
ASTM D790
Izod Impact, Notched 2.10 J/cm

@Thickness 3.18 mm,
Temperature -20.0 °C
3.93 ft-lb/in

@Thickness 0.125 in,
Temperature -4.00 °F
Injection Molded; ASTM D256A
8.00 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
15.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 105 °C

@Thickness 6.35 mm
221 °F

@Thickness 0.250 in
Unannealed; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 260 - 277 °C
500 - 531 °F
Mold Temperature 65.6 - 87.8 °C
150 - 190 °F
Drying Temperature 110 °C
230 °F
Dry Time 2.00 hour
2.00 hour
Descriptive Properties Value Comments
Features Good Weather Resistance
Forms Pellets
Generic Material PC+PBT
Generic Name Polycarbonate + PBT (PC+PBT)
Regional Availability Africa & Middle East