PolyOne Elastamax™ TM0200-0085 Black Thermoplastic Polyolefin Elastomer (TPO (POE))

Category Polymer , Thermoplastic , Elastomer, TPE , Olefinic TPE
Manufacturer PolyOne Corporation
Trade Name Elastamax™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Elastamax™ TM0200-0085 Black Thermoplastic Polyolefin Elastomer (TPO (POE)).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance of physical properties and processability, and are an economical alternative to traditional thermoset rubber and more costly thermoplastic elastomers.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
ASTM D792
Melt Flow 15 g/10 min
15 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 89
89
10 sec; ASTM D2240
Tensile Strength at Break 9.65 MPa
1400 psi
510 mm/min; ASTM D412A
Elongation at Break 700 %
700 %
510 mm/min; ASTM D412A
Izod Impact, Notched 2.90 J/cm
5.43 ft-lb/in
ASTM D256
Tear Strength 59.5 kN/m
340 pli
Die C, 510 mm/min; ASTM D624
Descriptive Properties Value Comments
Additive UV Stabilizer
Features General Purpose
Forms Pellets
Generic Material TPO (POE)
Generic Name Thermoplastic Polyolefin Elastomer (TPO (POE))
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Automotive Applications
Construction Applications
General Purpose
Industrial Applications