Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
ASTM D955
Spiral Flow 63.5 cm
25.0 in
Mechanical Properties Metric English Comments
Hardness, Shore D 81
81
ASTM D2240
Tensile Strength, Yield 49.6 MPa
7190 psi
Type I, 51 mm/min; ASTM D638
Tensile Modulus 3.03 GPa
439 ksi
Type I, 51 mm/min; ASTM D638
Flexural Strength 91.0 MPa
13200 psi
ASTM D790
Flexural Modulus 3.10 GPa
450 ksi
ASTM D790
Izod Impact, Notched 0.370 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.693 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
0.530 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.993 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 72.8 °C

@Thickness 6.35 mm
163 °F

@Thickness 0.250 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 72.2 °C

@Thickness 6.35 mm
162 °F

@Thickness 0.250 in
Unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 1.60 mm
V-0

@Thickness 0.0630 in
ALL; UL 94
Processing Properties Metric English Comments
Melt Temperature 199 - 210 °C
390 - 410 °F
Descriptive Properties Value Comments
Agency Ratings NSF 14
NSF 61
NSF Type I
Features Medium Flow
Forms Pellets
Generic Material PVC, Rigid
Generic Name Polyvinyl Chloride, Rigid (PVC, Rigid)
Processing Method Injection Molding
PVC Cell Classification 12454
ASTM D1784
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Fittings
Users viewing this material also viewed the following: