Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Rigid Extrusion 87768 Polyvinyl Chloride, Rigid (PVC, Rigid)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Rigid Extrusion 87768 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 81
81
15 sec; ASTM D2240
Tensile Strength, Yield 56.1 MPa
8140 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.65 GPa
384 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 99.9 MPa
14500 psi
ASTM D790
Flexural Modulus 3.33 GPa
483 ksi
ASTM D790
Izod Impact, Notched 3.70 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
6.93 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded; ASTM D256A
Dart Drop Total Energy 44.5 J/cm

@Temperature 23.0 °C
0.0834 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 67.0 µm/m-°C
37.2 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 57.8 °C

@Thickness 3.18 mm
136 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 179 °C
354 °F
Descriptive Properties Value Comments
Features High Gloss
Forms Pellets
Generic Material PVC, Rigid
Generic Name Polyvinyl Chloride, Rigid (PVC, Rigid)
Processing Method Coextrusion
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Capstock
Vertical Blinds
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved