Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Gravi-Tech™ GRV-TP-080-W-NAT Styrene Butadiene Block Copolymer (SBC)

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene-Butadiene Copolymer, SBC
Manufacturer PolyOne Corporation
Trade Name Gravi-Tech™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Gravi-Tech™ GRV-TP-080-W-NAT Styrene Butadiene Block Copolymer (SBC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 7.98 g/cc
7.98 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.020 cm/cm
0.020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 25
25
ASTM D2240
Tensile Strength, Yield 1.03 MPa
149 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 500 %
500 %
Type I, 5.1 mm/min; ASTM D638
Processing Properties Metric English Comments
Melt Temperature 163 - 204 °C
325 - 399 °F
Mold Temperature 15.6 - 37.8 °C
60.1 - 100 °F
Drying Temperature 76.7 °C
170 °F
Descriptive Properties Value Comments
Appearance Natural Color
Features High Specific Gravity
Non-Toxic
Forms Pellets
Generic Material SBC
Generic Name Styrene Butadiene Block Copolymer (SBC)
Processing Method Injection Molding
Regional Availability Asia Pacific
Uses Industrial Applications
Medical/Healthcare Applications
Projectiles
Sporting Goods
Weighting & Balancing