PolyOne Lubri-Tech™ PK-5GP/7T Polyetheretherketone (PEEK), PTFE Lubricated  (discontinued **)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Lubri-Tech™ PK-5GP/7T Polyetheretherketone (PEEK), PTFE Lubricated  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Graphite LubricatedPTFE LubricatedInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.393 g/cc
1.393 g/cc
ASTM D792
Water Absorption 0.20 %

@Thickness 3.17 mm
0.20 %

@Thickness 0.125 in
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0060 - 0.0080 cm/cm
0.0060 - 0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 89.6 MPa
13000 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 4.48 GPa
650 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 103 MPa
15000 psi
ASTM D790
Flexural Modulus 4.48 GPa
650 ksi
ASTM D790
Izod Impact, Notched 0.694 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.30 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256