Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Maxxam™ FR PP CONC 36 NAT S Polypropylene, Unspecified (PP, Unspecified)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer PolyOne Corporation
Trade Name Maxxam™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Maxxam™ FR PP CONC 36 NAT S Polypropylene, Unspecified (PP, Unspecified).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V-0, and 5VA performance ratings. In addition, many compounds in the Maxxam FR portfolio offer elevated Relative Thermal Index (RTI) ratings.MAXXAM FR PP CONC 36 NAT S is designed to impart good flame retardancy to polypropylene. Because there are so many varieties of polypropylene, it is difficult to predict the required let-down ratio required to meet the specific flammability standards. When the concentrate is let down at the proper ratio the resulting material can achieve flame retardancy equivalent to the requirements for UL94 V-2 or UL94 V-0. For starting point formulations we would suggest 7 to 8 parts by weight of polypropylene to 1 part of Conc 36 for UL94 V-2 performance and 2 to 3 parts by weight polypropylene to 1 part of Conc 36 for UL94 V-0 performance at thicknesses between 0.75 and 3.0 mm.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Melt Flow 70 g/10 min

@Load 2.16 kg,
Temperature 230 °C
70 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A; ASTM D1238
Descriptive Properties Value Comments
Features Flame Retardant
Forms Pellets
Generic Material PP, Unspecified
Generic Name Polypropylene, Unspecified (PP, Unspecified)
Regional Availability North America