Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Maxxam™ FR PP FR 8-6 A NATURAL - ROHS Polypropylene, Unspecified (PP, Unspecified)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer PolyOne Corporation
Trade Name Maxxam™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Maxxam™ FR PP FR 8-6 A NATURAL - ROHS Polypropylene, Unspecified (PP, Unspecified).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V-0, and 5VA performance ratings. In addition, many compounds in the Maxxam FR portfolio offer elevated Relative Thermal Index (RTI) ratings.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Melt Flow 2.5 - 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.5 - 5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 16.5 MPa
2390 psi
Type I, 51 mm/min; ASTM D638
Elongation at Break 80 %
80 %
Type I, 51 mm/min; ASTM D638
Flexural Strength 27.6 MPa
4000 psi
13 mm/min; ASTM D790
Flexural Modulus 1.38 GPa
200 ksi
ASTM D790
Izod Impact, Notched 2.10 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
3.93 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C

@Thickness 3.18 mm
185 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 0.750 mm
V-0

@Thickness 0.0295 in
All Color; UL 94
V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
All Colors; UL 94
V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
All Colors; UL 94
5VA

@Thickness 3.00 mm
5VA

@Thickness 0.118 in
All Colors; UL 94
5VA

@Thickness 2.20 mm
5VA

@Thickness 0.0866 in
All Colors; UL 94
Descriptive Properties Value Comments
Additive Impact Modifier
Features Flame Retardant
Impact Modified
Filler / Reinforcement Talc Filler
Forms Pellets
Generic Material PP, Unspecified
Generic Name Polypropylene, Unspecified (PP, Unspecified)
Regional Availability North America
RoHS Compliance Contact Manufacturer
Users viewing this material also viewed the following: