Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Nymax™ GF 1800 33 BLACK 13 Nylon 612 with 33% Glass Fiber  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 612 , Nylon 612, Glass Fiber Filler
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Nymax™ GF 1800 33 BLACK 13 Nylon 612 with 33% Glass Fiber  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Molded Test Bars: Dry as Molded
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Filler Content 33 %
33 %
Water Absorption 0.20 %

@Thickness 3.18 mm,
Time 86400 sec
0.20 %

@Thickness 0.125 in,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 148 MPa
21500 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 4.0 %
4.0 %
Type I, 5.1 mm/min; ASTM D638
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 1.01 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.89 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Melting Point 215 °C
419 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 193 °C

@Thickness 3.18 mm
379 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Descriptive Properties Value Comments
Appearance Black
Forms Pellets
Generic Name Polyamide 612 (Nylon 6/12)
Regional Availability North America
South America
Users viewing this material also viewed the following: