PolyOne Synprene® RT-4060 Thermoplastic Elastomer - SBC, Mineral Filled  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Synprene® RT-4060 Thermoplastic Elastomer - SBC, Mineral Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledApplications:Multi-PurposeMarket:AutomotiveBuilding and ConstructionIndustrialConsumer GoodsProcessing Method:ExtrusionInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Instant; ASTM D2240
Tensile Strength, Yield 5.93 MPa
860 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
3.79 MPa

@Strain 300 %
550 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 700 %
700 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Tear Strength 25.4 kN/m
145 pli
Die C (graves), 20 in/min; ASTM D624
Compression Set 20 %
20 %
Method B, 73°F(23°C), 22 hrs; ASTM D395